When porosity appears in die-cast parts, the usual response is to adjust shot speed, boost pressure or change the aluminum melt. These changes can help, but if the problem repeats, the machine is only one part of the picture.
Separate gas porosity from shrinkage porosity. Gas pores often have a smoother internal surface, while shrinkage cavities tend to appear in thicker sections and have an irregular shape. X-ray inspection, sectioning or microscopic examination can help identify the type. Treating every void as the same problem can lead to the wrong adjustment.
Die venting and gating are important. If air cannot escape, or the gate position does not fill the cavity in a suitable sequence, gas may be trapped. Over time, vent slots can become blocked by flash, release agent residue or aluminum particles. A die that worked well when new may need cleaning or vent maintenance.
Melt quality also matters. High temperature, incomplete degassing and a high gas content increase the risk of porosity. Changes in ingot source or the ratio of returns can shift the behavior. Keeping records of melt treatment and lot changes makes it easier to link a problem to a specific batch.
Shot parameters should match the die and the part. Low-speed and high-speed transition points, boost pressure, biscuit thickness and die temperature all affect air entrapment and feeding. Higher settings are not always better; the profile needs to work with the die design and cooling pattern.
Spraying is another variable. Uneven die temperature or excessive release agent can affect metal flow and leave gas or stains. Check nozzle position, spray time and die temperature at different locations.
Solving porosity usually means looking at die, melt, shot profile, cooling and spraying together. Identify the void type before changing the main variable, then track several production runs before deciding whether the improvement is stable.
Chinese